Structure and properties of high-strength steel connections under external static loading
Journal: Construction, materials science, mechanical engineering (Vol.1, No. 73)Publication Date: 2014-04-10
Authors : L. Markashova; V. Poznyakov; E. Berdnikov; T. Alekseenko; S. Zhdanov;
Page : 213-219
Keywords : Structure; HAZ; Fine-grained structures.;
Abstract
The research showed that the HAZ metal of welded joints, which made of high-strength steel 17Kh2M by welding wire Sv-10KhN2GSMFTYu with cooling rate W6/5 = 20ºC/s, has the high level of strength and fracture toughness as after welding as in the conditions of external load under 0,75∙σВ = 765 МРа and 0,85∙σВ = 867 МРа. This is ensured by the formation in the HAZ metal the maximum number of fine grain structures of the lower bainite and martensite vacation.
Other Latest Articles
- Analysis of fracture mechanisms sheets from low carbon, low alloy steels under static and dynamic loads. Chapter
- Features crystallographic relations between the lattices of the primary and eutectoid ferrite
- Prospects of development information and control systems yzmerytelnoy la spatial orientation objects
- Analysis of the dependence of the mechanical properties of HSLA steels of hot rolling temperature and deformation parameters
- Effect velychynы grain and other factors on the dispersion of carbonaceous pearlite steels
Last modified: 2017-04-23 06:26:42