EFFECT OF FINELY-DISPERSED COAL SLUDGES ON THEIR FLOATABILITY
Journal: Scientific and Technical Journal of Information Technologies, Mechanics and Optics (Vol.19, No. 5)Publication Date: 2019-10-01
Authors : V.N. Petukhov N.Yu. Svechnikova O.V. Kuklina A.S. Puzina T.N. Akhmetzyanov Ya.V. Gavryushina;
Page : 840-847
Keywords : flotation; fine-dispersed coal particles; adsorption; physicochemical properties; flocculation;
Abstract
Subject of Research. We study the effect of physical and chemical properties of finely-dispersed coal sludges of “MMK-UGOL” on their floatability. Method. Petrographic analysis of coal was carried out using the analyzer of petrographic properties of SIAMS 620 coal. To identify the presence of the main functional groups in the macromolecule of the organic mass of coal, the method of automated analysis of coal by infrared reflection spectra (IR-spectrum) was used. The electrical conductivity of the pulp with a crushed coal sample was determined by ANION 4100 liquid analyzer. Flotation studies were carried out in laboratory flotation machine of FML-1 type (Research and Production Company “Mechanobr-Technika”, Russia). Main Results. The action mechanism of new reagents in the flotation of finely-dispersed coal sludges has been identified. The flocculating action of “Sinterol” new reagent on the mineral particles of finely-dispersed coal sludges has been elucidated, that improves significantly the selectivity of the flotation process. The optimum flotation mode of thin coal sludges has been developed on the basis of laboratory researches, which increases resource efficiency of coal enrichment technological process due to the decrease in organic weight loss with waste by 33%. Thus, the consumption of the consumed reagents is reduced by 3 times. Practical Relevance. The efficiency of “Sinterol” reagent-flocculant has been confirmed by industrial tests on JSC MMK-COAL (Russia). Thus when applying “Sinterol” reagent- flocculant in the flotation process in an amount of 0.001–0.003 kg/t and simultaneously reducing the total consumption of reagents by an average of 13.0% from 3.000 to 2.613 kg/t, the concentrate yield has increased by 2.5–8.5%, the ash content of the concentrate has decreased by 2.7–3.0%, while the ash content of waste has increased by 2.9–12.3%.
Other Latest Articles
- GEOMETRICAL SYNTHESIS METHOD AND PARAMETRIC OPTIMIZATION OF GALLOPING ROBOT LEG MECHANISM
- EFFECT OF OBJECT REPRESENTATION FORM ON DEPTH RESOLUTION OF RESTORED IMAGES OBTAINED BY SYNTHESIZED FRESNEL HOLOGRAMS
- ROTATION PARAMETER ESTIMATION ERROR OF DEFLECTOMETER BASIC UNIT
- ULTRASOUND DETECTION BY APPLYING FIBER BRAGG GRATINGS
- Kyiv archpriest Ioann Levanda and his library in the funds of Vernadsky National Library of Ukraine
Last modified: 2019-10-23 19:21:48