The Influence of the Deposition Rate of Application on the Thickness of the Molybdenum Layer
Journal: Agricultural, Forest and Transport Machinery and Technologies (Vol.6, No. 1)Publication Date: 2019-12-01
Authors : Marian Bujna; Plamen Kangalov; Mitko Nikolov;
Page : 38-43
Keywords : molybdenum layer; thermal spraying; exceeded thickness; quality production;
Abstract
Our research was based on the requirements of practice. The production organization asked us to solve the problem of application of molybdenum layer thermal spraying. In some samples, a large thickness was measured, making it impossible to produce the product of the required parameters. The product was a molybdenum lamella for brakes and clutches. The rate of application should be constant throughout the production of the lamella. Exceeded thickness is caused by the use of a large volume of additive material. Molybdenum is a very expensive metal, which ultimately results in a financial loss. In the paper we reviewed various causes of this problem and their onsequences. Based on the research, we determined that the main cause of the large thickness of the applied layer was the non-compliance with the constant molybdenum wire feed rate. We have taken corrective measures to prevent it from happening again. Linking with practice and handling manufacturers' problems is very important for our research.
Other Latest Articles
- Resistance of Nickel-Plated Components
- Resistance of Components to Zinc Plated Against Corrosion
- Analysis of Quality Management System Audit in a Selected Organization
- ENVIRONMENTAL IMPACT FROM METALURGJIK COMPLEX ``TREPÇA`` IN AREA OF MITROVICA
- ASSESMENT OF THE HEAVY METALS PRESENCE IN THE WATER, SOIL AND LANDFILL OF THE DRENICA RIVER – NEARBY THE INDUSTRIAL BY COMPLEX FERRONICKEL
Last modified: 2020-02-09 03:18:19