Synthesis and Specific Absorption Rate of Fe3O4 Nanoparticles
Journal: International Journal of Science and Research (IJSR) (Vol.4, No. 2)Publication Date: 2015-02-05
Authors : E. I. A. Elbeshir;
Page : 932-934
Keywords : Magnetic nanoparticles; hyperthermia;
Abstract
The sample of Fe3O4 magnetic nanoparticles (MNPs) are synthesized via co-precipitation method from ferrous and ferric solutions. X-ray diffraction (XRD) used to characterized the powder synthesized of Fe3O4. The average lattice parameter and the average size of Fe3O4 MNPs were a = 8.3 and t = 9.12 nm. Induction heater operated at low frequencies 100 kHz was used to study the heating rate (T/t oC/ sec) and the specific absorption rate (SAR W. g -1) of the Fe3O4 MNPs and were found to be 0.025 oC/ sec and 105 W. g -1 respectively.
Other Latest Articles
- Mobility Prediction with Minimum Energy Consumption
- Performance of ICI Cancellation in OFDM System Using Different Reduction Techniques
- Studies on Diethanolaminedithiocarbamate as Metal Complex, Complexing Agent and Stabilizer in Copper Methanesulphonate Bath
- Comparative Study on Content Based Image Retrieval Based on Color, Texture (GLCM&CCM) Features
- Enhancement of ECG Signal by using Digital FIR Filter
Last modified: 2021-06-30 21:22:46