Minimizing Friction between Die and Punch using Ferro Fluids in Pressure Compaction of Metal Powder
Journal: International Journal of Science and Research (IJSR) (Vol.4, No. 11)Publication Date: 2015-11-05
Authors : Akshansh Mishra; Anand Singh;
Page : 1772-1773
Keywords : Friction; die; punch; Ferrofluid; Alnico;
Abstract
During the last twenty years powder metallurgy has progressed in many new direction, new types of products have been manufactured and new method of manufacturing have been developed. One of those method is pressure compaction method in which blended powder are pressed into shape in die with the help of punch. So there is some friction between punch and die during this operation. Hence in order to overcome that friction we are using Ferrofluid to prevent the damage occurred due to friction in punch and die.
Other Latest Articles
- Supply Chain Model on Uncertainty Demand
- Secondary School Writing Errors at White Nile State Sudan: A Case Study of Assalaya Locality
- Impact of Social Media Marketing on Business Exposure and Customer Response: A Study on Educational Institutes of Chhattisgarh
- Recommendations to Evaluate and Choose Cloud Services and Deployment Models for e-Business Strategic Use: A Case Study of Malaysian SMEs
- Implicit Sentiment Identification using Aspect based Opinion Mining
Last modified: 2021-07-01 14:26:37