Abstract
Meta phenylenediamine 4 sulphonic acid (MPDSA) is one of the important products in the dyestuff sector. The present conventional manufacturing process for MPDSA being carried out at the industry is less efficient and gives an overall yield of about 60 %. But the use of alternative raw materials for the manufacture of MPDSA can give yield as high as upto 80%. In addition , this process also eliminates the use of metal catalysts which cause downstream problems. This method involves the use Metaphenylene Diamine as the raw material instead of 2, 4, dinitrochlorobenzene for the manufacture of MPDSA. A lab scale experiment has been carried out and the overall yield has been found to be higher than that obtained from the conventional process. This paper describes this new manufacturing process and its possible economic benefits. Overall yield is calculated and compared with the conventional process.
Other Latest Articles
- Recognition Capability of ANN For The Analysis of PbO-Doped Sno2 Sensor For Detection of Acetone
- Process Modification in Dye and Dye Intermediates ? Acid Dyes
- Wireless Transmission Network : A Imagine
- Convective Heat and Mass Transfer Flow from a Vertical Surface with Radiation, Chemical reaction and Heat Source/Absorption
- Review of Heat Transfer Augmentation Within A Plate Heat Exchanger By Different Shapes Of Ribs
Last modified: 2013-05-24 22:09:23