Effect of Sand to Fly Ash Ratio on the Hardened Properties of Geopolymer Mortar
Journal: International Journal of Computational Engineering Research(IJCER) (Vol.6, No. 9)Publication Date: 2016-09-30
Authors : Supratim Guha; Srijita Dey; Prakash Sarkar; Arindam Routh;
Page : 48-56
Keywords : Alkaline solution; Compressive strength; Fly ash; Geopolymer mortar; Sorptivity; Water absorption;
Abstract
This paper presents the progress of research on making Geopolymer mortar using the fly ash obtained from Kolaghat Thermal Power Station, (KTPS), Kolaghat, India. This paper results the report of the experimental study on mechanical property in terms of compressive strength that tested after heat curing in oven by varying fly ash to sand ratio 1:1 to 1:3. Sodium Hydroxide was used as alkali activator in this process. The two main parameters are .Synthesis parameter, i.e. alkali content, sand to fly ash ratio in geopolymer mixture, and Processing parameters i.e. mixing time, curing time, curing temperature to develop the compressive strength was studied. The test results show that, by increasing the sand to fly ash ratio compressive strength decreases. Again this feature was further backed up by typical properties like Water absorption, Sorptivity & Apparent Porosity
Other Latest Articles
- Essential and organizational transformations of economy management in the countryside as the basis of sustainable rural development in Ukraine
- Bicycle transport as an object of ecological marketing and innovations in urban transportations
- Problems of export orientation of Ukrainian industrial enterprises
- Analysis of the foreign economic factors impact on the welfare of Ukrainians in the conditions of the world integration processes
- Indicators of science that are critical for creation of Ukrainian research universities
Last modified: 2016-10-06 13:33:38