The impact of hardening from inter-critical temperature interval (ITI) and subsequent high tempering on the structure and properties of steels 40HN and 40HN2MA
Journal: Reporter of the Priazovskyi State Technical University. Section: Technical sciences (Vol.26, No. 1)Publication Date: 2013-06-13
Authors : L.S. Malinov; D.V. Burova;
Page : 93-99
Keywords : inter-critical temperature interval; martensite; ferrite; metastable austenite; hardening; high tempering; mechanical properties;
Abstract
The results of research on getting good combination of mechanical properties of steel 40HN and 40HN2MA by heat treatment were presented, which include heating in inter-critical temperature interval (ITI),which create heterogeneous multiphase structure in them
Other Latest Articles
- The particularities of manganese distribution in high-chromium cast irons
- Regularities and mechanisms of corrosion dissolution of steel AISI 321 in weak acid chloride solution
- The influence of the quantity and the stability of retained austenite on wear resistance and mechanical properties of steels with 18% Cr
- The effect of alloying with secondary material upon carbide phase steel 3X2B8Ф
- A Conceptual Study on Supply Chain Management in Creating Customer Value
Last modified: 2015-07-29 18:37:36