Abstract
The Study aimed at improving the quality of chrome-tanned leather for golf floves producted by Indonesian tanners. Samples used in this study were 32. They were visually inspected and tested on their chemical and physical properties. The results of the chemical and physical tests were analyzed using deviation standard in descriptive statistics. It was obtained from the visual inspection of the samples taken that the leather was soft enough, the colour was even, their hair was not loose, and it was flexible but not elastic. While from the Chemical Tests, the results obtained were : water content (13,78 ? 16,94) %; Fat Content (6,04 ? 11,38) % and pH Valueness (4,43 ? 5,19). It was obtained from the physical tests that Thickness (0,32 ? 0,64) mm; well tanned; Tensile Strength resistence (106,07 ? 109,73) kg/cm2; Flexibility (53,11 ? 103,07) %; Slit Tear Resistance (13,48 ? 39,22) kgf/cm; Stitch Tear Strength (74,51 ? 137,79) kgf/cm, wet rub fastness tst shown a little discolourisation while dry rub fastness test shown no discolourisation.
Other Latest Articles
- Methodology and key determinants of building an efficient national innovation system of a country
- Investment activity in the Visegrad countries: challenges for Ukraine
- Analysis of world’s trends of bankruptcy and Ukrainian realities as a recall to the global instability
- Globalization, crises and policy reform: lessons from the Turkish experience
- Economic growth and military expenditure linkages: a panel data analysis
Last modified: 2016-02-12 10:54:51